| Specification |
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance, Excellent Thermal Shock Resistance;
Production Process: Fusion Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Powder;
Product Name: Corundum Mullite Castable;
Application Limit Temp: 1400-1800℃;
Type: Monolithic Refractory Material;
CCS/Mor: 14-60MPa;
Keyword: High Strength Castable Refractory;
Bulk Density: 2.0-2.9g/cm3;
Thermal Conductivity: 0.6-1.1W/M.K;
Sio2: 10-55%;
Package: Sea-Worthy Wooden Pallet+Woven B;
Certifiacte: ISO9001, CE, etc;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|