| Specification |
Feature: Long Time Materials, Instant Materials, Firebrick;
Refractoriness (℃): Refractoriness> 2000;
Shape: Block;
Product Name: Chrome Corundum Refractory Brick;
Apparent Porosity: 20.0-22.0;
Bulk Density(Kg/M3): 2.9-3.8g /Cm3;
Cold Crushing Strength(MPa): 40~70MPa;
Advantage: Thermal Shock Resistance;
Keyword: Refractory Chrome Corundum Brick;
Application: Blast Furnace, Glass Kiln, Cement Kiln and So on;
Al2O3 Content (%): 48%-85%;
Raw Material: Zircon Sand;
Processing Service: Punching, Cutting, Moulding;
Type1: Fire Brick;
Type: Heat-Resistant Material;
Material: China High Alumina Brick;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|