| Specification |
Material: Recrystallized Silicon Carbide;
Refractoriness (℃): Under 1620 Deg C (Oxid);
Shape: Batts/Setters/Plate/Setting Ring, etc.;
Density: 2650-2750 Kg/M3;
Customized Shape: Yes;
Features: Heavy Loading Weight, Low Weight, High Temperature;
Thermal Shock Resistant: Extremely;
Application: Porcelain Sanitary Ware/Metal Powder Process, etc.;
Feature: Long Time Materials, Instant Materials;
Type: Refractory Material;
|
Material: Silicon Carbide (SiC);
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Powder, Particle / Powder;
Application: Abrasive Tools, Refractory, Ceramics, etc;
Color: Black / Green;
Other Name: Carborundum, Emery;
Abrasive Grain Sizes: 0-1, 1-3, 3-5, 0-10mm, F12-F220, Customized;
Feature: Long Time Materials;
Type: Semi-Conductor Non-Metal;
|
Material: Zircon, Zirconia;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Plate;
Usage: Melting;
Name: High Temperature Refractory Corundum Crucible for;
Volume: 5-2000ml;
Size: Customized Is Ok;
Color: White;
Keyword1: Zro2 Tray;
Keyword2: Zirconia Ceramic Sagger;
Keyword3: Zro2 Ceramic Sagger;
Keyword4: Ceramic Tray;
Feature: Long Time Materials;
Type: Refractory Material;
|
Material: Pure Zirconium;
Refractoriness (℃): Refractoriness> 2000;
Shape: Plate;
Usage: Aerospace, Ceramic Production, Chemical Industry, Environmental Protection Equipment, Glass Manufacturing, Industrial Kilns, Petroleum Refining, Steel Smelting;
Zirconium Content: Zirconium Content>65%;
Working Temperature: 1050c/1260c/1400c;
Manufacturer: Redon;
Other Name: Rd's Ceramic Fiber Board Refractory Material;
Mean Diameter: 200nm-400nm/800nm-1um/2-4um;
Fibrous Phase: Tetragonal;
|
Material: Zirconia-Corundum;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Block;
Usage: Aerospace, Environmental Protection Equipment, Glass Manufacturing, Industrial Kilns, Steel Smelting;
Feature: Long Time Materials;
Type: Refractory Material;
Size: Customizable;
Certifiacte: ISO9001, CE, etc;
Apparent Porosity: 1.3-2.0%;
Bulk Density: 3.4-4.0g/cm3;
Cold Crushing Strength: 350MPa;
Thermal Linear Expansion(%): 0.8;
Zro2: 32-40%;
Na2o: 1.3-1.5%;
Sio2: 13-15.5%;
|