| Specification |
Usage: High Temperature Insulating Material;
Temprature Classification: 1900℃, 1600℃, 1500℃, 1400℃, 1260℃, 1050℃, as Requested;
Chemical Composition:: SiO2, Al2sio5;
Shape: Ceramic Fiber Heating Module;
Manufacturing Technique: Standard Process;
Kind: High Purity Ceramic Fiber;
|
Usage: Iron Voltage Electric Material, Thermal Insulation Coatings, Packing Material, High Temperature Insulating Material;
Temprature Classification: 1600℃, 1500℃, 1400℃, 1260℃, 1050℃;
Chemical Composition:: SiO2, Al2O3.SiO2, Al2O3;
Shape: Ceramic Fiber Blanket;
Manufacturing Technique: Spray Silk Rug;
Kind: Ordinary Ceramic Fiber;
Customization: Available;
Al2O3: 44-47;
Thermal Conductivity: 0.153;
Shot Content: 15;
|
Usage: Iron Voltage Electric Material, Thermal Insulation Coatings, Packing Material, High Temperature Insulating Material;
Temprature Classification: 1600℃, 1500℃, 1400℃, 1260℃, 1050℃;
Chemical Composition:: SiO2, Al2O3.SiO2, Al2O3;
Shape: Ceramic Fiber Blanket;
Manufacturing Technique: Spray Silk Rug;
Kind: Ordinary Ceramic Fiber;
Customization: Available;
Al2O3: 43;
Thermal Conductivity: 0.153;
Shot Content: 15;
|
Usage: Iron Voltage Electric Material, Thermal Insulation Coatings, Packing Material, High Temperature Insulating Material;
Temprature Classification: 1600℃, 1500℃, 1400℃, 1260℃, 1050℃;
Chemical Composition:: SiO2, Al2O3.SiO2, Al2O3;
Shape: Ceramic Fiber Blanket;
Manufacturing Technique: Spray Silk Rug;
Kind: Ordinary Ceramic Fiber;
Customization: Available;
Al2O3: 40;
Thermal Conductivity: 0.153;
Shot Content: 15;
|
Usage: Iron Voltage Electric Material, Thermal Insulation Coatings, Packing Material, High Temperature Insulating Material;
Temprature Classification: 1500℃, 1400℃, 1260℃, 1050℃;
Chemical Composition:: SiO2, Al2O3.SiO2, Al2O3;
Shape: Ceramic Fiber Cotton;
Manufacturing Technique: Spray Silk Rug;
Kind: Ordinary Ceramic Fiber;
Color: White;
Customization: Available;
Al2O3: 43-45;
|