| Specification |
Feature: Corrosion Resistance, Good Insulation Performance, Thermal Shock Resistance;
Production Process: Pressing Method;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Plate;
Al2O3 %: 85%;
C%: 2.5%;
B.D(≥g/cm3): 2.9;
a.P.P(≤%): 12;
C.C.S(≥MPa): 100;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|