| Specification |
Feature: Corrosion Resistance, Good Insulation Performance, Thermal Shock Resistance;
Production Process: Sintering Method;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Plate;
Al2O3 %: 85%;
C%: 2.5%;
B.D(≥g/cm3): 2.9;
a.P.P(≤%): 12;
C.C.S(≥MPa): 100;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, Good Thermal Shock Resistance;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Rectangle, Cylindrical, Round, Sagger;
Usage: Kiln Furniture, Roller Kiln, Ovens or Kilns;
Size: 330*300*100 or Customized;
Temperature: 1000-1400c;
Material: Porcelain;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, Good Thermal Shock Resistance;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Rectangle, Cylindrical, Round, Sagger;
Usage: Kiln Furniture, Roller Kiln, Ovens or Kilns;
Size: 330*300*100 or Customized;
Temperature: 1000-1400c;
Material: Porcelain;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance;
Production Process: Fusion Method;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Plate;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance;
Production Process: Fusion Method;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Plate;
|