| Specification |
Application: Aerospace, Electronics, Medical, Refractory, Semiconductor, National Defense, Industrial;
Density: >3.0 g/cm�;
Material: Silicon Carbide;
Color: Dark Grey;
Flexural Strength: 350-450 MPa;
Thermal Conductivity: 80-120 W/Mk;
Max Working Temperature: 1380-1750 C;
Corrosion Resistance: Corrosion Resistant;
Thermal Stability: Extreme Temperature Stability;
Hardness: 9 Mohs;
Type: Ceramic Part;
|
Application: Refractory, Industrial Ceramics;
Density: High Density;
Material: Alumina;
Shape: Arc, Conical, Cylinderical, Tubular, Tall Form;
Strength: High Strength;
Pressing Speed: Punch Forming;
Suppression Method: Unidirectional Pressurization;
Color: Ivory, Cream, White, Pink Color;
Advantage: High Temperature and Chemical Corrosion;
Working Temperature: 1600c, 1700c, 1800c;
Purity: 95% 99%;
Type: Ceramic Part;
Size Tolerance: Tight;
Surface Finish: Normal,Polished, Mirror Polished ,Diamond Polished;
Surface: Ra 0.4,Ra 0.2;
|
Application: Refractory Lining, Thermal Insulation, Industrial Applications;
Density: >6.0g/Cm³;
Material: Zirconia;
Shape: Ring;
Strength: High Strength;
Customization: Available;
Sample: Available(The Smallest Size);
Features: Wear, Corrosion and Heat Resistant;
Hardness: >87hra;
Type: Ceramic Part;
Flexural Strength: >950MPa;
Purity: 94.8%Zr02, 5.2%Y203;
|
Application: Catalytic Converter, Heat Exchanger, Refractory Lining, Thermal Insulation;
Density: High Density;
Material: Zirconia;
Shape: Tube;
Strength: High Strength;
Customization: Available;
Sample: Available(The Smallest Size);
Features: Wear, Corrosion and Heat Resistant;
Hardness: >87hra;
Type: Ceramic Part;
Flexural Strength: >950MPa;
Purity: 94.8%Zr02, 5.2%Y203;
|
Application: Catalytic Converter, Heat Exchanger, Refractory Lining, Thermal Insulation;
Density: High Density;
Material: Zirconia;
Shape: Tube;
Strength: High Strength;
Customization: Available;
Sample: Available(The Smallest Size);
Features: Wear, Corrosion and Heat Resistant;
Hardness: >87hra;
Type: Ceramic Part;
Flexural Strength: >950MPa;
Purity: 94.8%Zr02, 5.2%Y203;
|