| Specification |
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance;
Production Process: Casting High Temperature Firing;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Block;
Product Name: Refractory Purge Plug for Ladle Bottom Argon PUR;
Type 1: Slit/Slot Type Purge Plug;
Type 2: Porous Purge Plug;
Type 3: Segment /Plate Purge Plug;
Type 4: Preassembled Purge Plug and Well Block;
Types: Cleaning Plugs and Related Systems;
Metallurgical Needs: Different Refining Processes (Rh, Lf, Vd, VOD, Va;
Raw Material of Slit Type: Chromite Corundum Spinel or Corundum Spinel;
Main Feature: High Blowing Rate;
Advantage: Easyier for Operation Control During Refining Proc;
Flow Rate Range: 12%-20%;
Al2O3/(%) Content: Not Less Than 85%;
Al2O3+MGO+Cr2o3 /(%): Not Less Than 93%;
Bubulk Density/(g/cm3): Not Lower Than 3.0;
Application: Core Components for Refining and Post-Furnace Trea;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|