| Specification |
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Abrasion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point, Thermal Shock Resistance;
Production Process: Sintering Method;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Plate;
Product Name: Ls70 Ladle Slide Gate;
Material: Al-Zr-C or Al-C;
Brand: Sinorefractory /Snref;
Main Element: Alumina&Zirconia&Carbon;
Application: Ladle of Steel Mill;
Process: Shaped-Dry-High Temperature Firing-Pitch Immersed-;
Flatness of Sliding Surface: Less Than 0.05mm;
Feature 1: High Mechanical Strength;
Feature 2: High Resistance;
Feature 3: Excellent Oxidation Resistance;
Feature 5: Good Thermal Shock Stability;
Service Life: 4-8 Heats;
Usage Area: Continuous Casting in Steel Plant;
Workmanship: High Temperature Deep Burnt;
Other Material Type: Al-C or MGO Spinel Slide Plates;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, Good Thermal Shock Resistance;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Rectangle, Cylindrical, Round, Sagger;
Usage: Kiln Furniture, Roller Kiln, Ovens or Kilns;
Size: 330*300*100 or Customized;
Temperature: 1000-1400c;
Material: Porcelain;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: 55% 60% 70%;
Compressive Strength MPa: 10,15,15;
Bulk Density g/cm3: 2.5 2.6 2.7;
Flexural Strength MPa: 3.0 4.0 4.0;
Refractoriness℃: ≥1750;
Si+C (%): 12_15;
|
Feature: Chemical Corrosion Resistance, Corrosion Resistance, Good Insulation Performance, High Mechanical Strength, High Melting Point;
Production Process: Sintering Method;
Refractoriness (℃): Refractoriness> 2000;
Shape: Powder;
Ai2o3%: ≥85;
Compressive Strength MPa: 1400,50;
Bulk Density g/cm3: 2.8;
Flexural Strength MPa: 1400,10;
|