| Specification |
Classification: Stainless Steel;
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Low Thermal Conductivity, Long Time Materials;
Production Process: Sintering Method;
Refractoriness (℃): 1580< Refractoriness< 1770;
Shape: Customized;
Raw Material: Stainless Steel SS304 Ss310;
Certifiacte: ISO9001, CE, etc;
Feature 2: High Hardness, High Thermal Shoc;
Working Temperature: 1200~1700℃;
Application: Industrial Furnace;
Thermal Shock Resistance: Excellent;
Refractoriness: 1500-1800 ℃;
Refractoriness Under Load (0.2MPa): 1350-1700 ℃;
Color: Silver;
Size Control: Accurate;
Production Time: 15-30 Days;
Testing Laboratory: Support;
|
Classification: High-Alumina;
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Square;
Volume: 1000ml;
Temperature: 1600~2000c;
Purity: 99%;
Density: Over 3.65g/cm3;
Secondary Process: Fine Grinding, CNC Machining;
Features: High Precision, High Insulation;
Usage: High-Temperature Ceramic Crucible;
Refractoriness: 1580< Refractoriness< 1770;
Weight: 0.2kg;
Melting Point: 2020℃;
Flexural Strength: 145-354MPa;
Hardness: 5.7-12.3gpa;
Elastic Modulus: 120-205gpa;
Thermal Conductivity: 2.5-25W/(M.K);
Poissons Ratio: 0.21-0.30;
|
Classification: High-Alumina;
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Square;
Volume: 1000ml;
Temperature: 1600~2000c;
Purity: 99%;
Density: Over 3.65g/cm3;
Secondary Process: Fine Grinding, CNC Machining;
Features: High Precision, High Insulation;
Usage: High-Temperature Ceramic Crucible;
Refractoriness: 1580< Refractoriness< 1770;
Weight: 0.2kg;
Melting Point: 2020℃;
Flexural Strength: 145-354MPa;
Hardness: 5.7-12.3gpa;
Elastic Modulus: 120-205gpa;
Thermal Conductivity: 2.5-25W/(M.K);
Poissons Ratio: 0.21-0.30;
|
Classification: High-Alumina;
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Square;
Volume: 1000ml;
Temperature: 1600~2000c;
Purity: 99%;
Density: Over 3.65g/cm3;
Secondary Process: Fine Grinding, CNC Machining;
Features: High Precision, High Insulation;
Usage: High-Temperature Ceramic Crucible;
Refractoriness: 1580< Refractoriness< 1770;
Weight: 0.2kg;
Melting Point: 2020℃;
Flexural Strength: 145-354MPa;
Hardness: 5.7-12.3gpa;
Elastic Modulus: 120-205gpa;
Thermal Conductivity: 2.5-25W/(M.K);
Poissons Ratio: 0.21-0.30;
|
Classification: High-Alumina;
Feature: Good Mechanical Strength, Good Thermal Insulation Performance, High-Temperature Resistant, Light Weight, Low Thermal Conductivity;
Production Process: Sintering Method;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Square;
Volume: 1000ml;
Temperature: 1600~2000c;
Purity: 99%;
Density: Over 3.65g/cm3;
Secondary Process: Fine Grinding, CNC Machining;
Features: High Precision, High Insulation;
Usage: High-Temperature Ceramic Crucible;
Refractoriness: 1580< Refractoriness< 1770;
Weight: 0.2kg;
Melting Point: 2020℃;
Flexural Strength: 145-354MPa;
Hardness: 5.7-12.3gpa;
Elastic Modulus: 120-205gpa;
Thermal Conductivity: 2.5-25W/(M.K);
Poissons Ratio: 0.21-0.30;
|