| Specification |
Material: Zircon, Alumina;
Refractoriness (℃): 1580< Refractoriness< 1770;
Usage: Tundish;
Zirconium Content: Zirconium Content>65%;
Feature 1: High Purity, High Density, Longer Working Life;
Feature 2: Strong Resisting Alkaline of Steel Liquid and Slag;
Feature 3: Strong Resisting Steel Liquid Crushing;
|
Material: Zircon;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Customized;
Usage: Aerospace, Ceramic Production, Chemical Industry, Environmental Protection Equipment, Glass Manufacturing, Industrial Kilns, Petroleum Refining, Steel Smelting;
Zirconium Content: 30%<Zirconium Content<65%;
Appearance: White, Rigid, Smooth Surface, No Damage;
Recommended Maximum Service Temperature: 1800-2200;
Crystalline Phase: Cubic Zro2;
Permanent Linear Change (1600°C × 2h, %): 0.1-0.5;
|
Material: Zircon;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Customized;
Usage: Aerospace, Ceramic Production, Chemical Industry, Environmental Protection Equipment, Glass Manufacturing, Industrial Kilns, Petroleum Refining, Steel Smelting;
Zirconium Content: 30%<Zirconium Content<65%;
Appearance: White, Rigid, Smooth Surface, No Damage;
Recommended Maximum Service Temperature: 1800-2200;
Crystalline Phase: Cubic Zro2;
Permanent Linear Change (1600°C × 2h, %): 0.1-0.5;
|
Material: Zircon;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Customized;
Usage: Aerospace, Ceramic Production, Chemical Industry, Environmental Protection Equipment, Glass Manufacturing, Industrial Kilns, Petroleum Refining, Steel Smelting;
Zirconium Content: 30%<Zirconium Content<65%;
Appearance: White, Rigid, Smooth Surface, No Damage;
Recommended Maximum Service Temperature: 1800-2200;
Crystalline Phase: Cubic Zro2;
Permanent Linear Change (1600°C × 2h, %): 0.1-0.5;
|
Material: Zircon;
Refractoriness (℃): 1770< Refractoriness< 2000;
Shape: Customized;
Usage: Aerospace, Ceramic Production, Chemical Industry, Environmental Protection Equipment, Glass Manufacturing, Industrial Kilns, Petroleum Refining, Steel Smelting;
Zirconium Content: 30%<Zirconium Content<65%;
Appearance: White, Rigid, Smooth Surface, No Damage;
Recommended Maximum Service Temperature: 1800-2200;
Crystalline Phase: Cubic Zro2;
Permanent Linear Change (1600°C × 2h, %): 0.1-0.5;
|